Internal oxidation of Ni-Cr-Al alloys under various oxygen partial pressures at 1273 K

Alloys for high temperature application always rely on their ability to form protective, dense Cr2O3 and Al2O3 scales. In case of Ni-Cr binary alloy, a minimum composition of Cr is required for the formation of continuous protective scale. However, addition of small amount of third element such as A...