Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique

ZnO thin films were fabricated on glass substrate by sol-gel method. A stable and homogeneous solution was prepared by dissolving zinc acetate dehydrate as a starting material in a solution of 2-methoxyethanol and monoethanolamine (MEA). The precursor concentration was selected as the parameter to o...

全面介紹

書目詳細資料
發表在:AIP Conference Proceedings
主要作者: 2-s2.0-79961098768
格式: Conference paper
語言:English
出版: 2011
在線閱讀:https://www.scopus.com/inward/record.uri?eid=2-s2.0-79961098768&doi=10.1063%2f1.3586950&partnerID=40&md5=9b1d27152372ad36750e40040cfe9ada
id Malek M.F.B.; Mamat M.H.B.; Zahidi M.B.M.; Sahdan Z.B.; Khusaimi Z.B.; Mahmood M.R.B.
spelling Malek M.F.B.; Mamat M.H.B.; Zahidi M.B.M.; Sahdan Z.B.; Khusaimi Z.B.; Mahmood M.R.B.
2-s2.0-79961098768
Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
2011
AIP Conference Proceedings
1342

10.1063/1.3586950
https://www.scopus.com/inward/record.uri?eid=2-s2.0-79961098768&doi=10.1063%2f1.3586950&partnerID=40&md5=9b1d27152372ad36750e40040cfe9ada
ZnO thin films were fabricated on glass substrate by sol-gel method. A stable and homogeneous solution was prepared by dissolving zinc acetate dehydrate as a starting material in a solution of 2-methoxyethanol and monoethanolamine (MEA). The precursor concentration was selected as the parameter to optimize the thin films quality. The molar ratio of zinc acetate dehydrate was kept at 1. The thin films were preheated at 300°C for 10 minutes after each coating. After depositing all layers, the thin films are annealed for 1 hour in order to obtain transparent ZnO thin films. It was found that the precursor concentration affect the IV characteristic, transmittance, and the thickness of the resultant ZnO thin films. © 2011 American Institute of Physics.

15517616
English
Conference paper

author 2-s2.0-79961098768
spellingShingle 2-s2.0-79961098768
Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
author_facet 2-s2.0-79961098768
author_sort 2-s2.0-79961098768
title Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
title_short Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
title_full Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
title_fullStr Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
title_full_unstemmed Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
title_sort Electrical and optical properties of zinc oxide thin films by sol-gel dip-coating technique
publishDate 2011
container_title AIP Conference Proceedings
container_volume 1342
container_issue
doi_str_mv 10.1063/1.3586950
url https://www.scopus.com/inward/record.uri?eid=2-s2.0-79961098768&doi=10.1063%2f1.3586950&partnerID=40&md5=9b1d27152372ad36750e40040cfe9ada
description ZnO thin films were fabricated on glass substrate by sol-gel method. A stable and homogeneous solution was prepared by dissolving zinc acetate dehydrate as a starting material in a solution of 2-methoxyethanol and monoethanolamine (MEA). The precursor concentration was selected as the parameter to optimize the thin films quality. The molar ratio of zinc acetate dehydrate was kept at 1. The thin films were preheated at 300°C for 10 minutes after each coating. After depositing all layers, the thin films are annealed for 1 hour in order to obtain transparent ZnO thin films. It was found that the precursor concentration affect the IV characteristic, transmittance, and the thickness of the resultant ZnO thin films. © 2011 American Institute of Physics.
publisher
issn 15517616
language English
format Conference paper
accesstype
record_format scopus
collection Scopus
_version_ 1828987884147834880