Performance of Permeable Concrete Pavement Containing Recycled Aggregate

Permeable pavement is a form of concrete pavement with a high porosity that allows water from precipitation and other sources to pass through directly, decreasing runoff and permitting groundwater recharging. It is used for concrete flatwork applications. The aim of this study is to evaluate the per...

Full description

Bibliographic Details
Published in:AIP Conference Proceedings
Main Author: Liew S.I.N.; Ng C.M.; Hasan M.; Jaya R.P.; Masri K.A.; Shaffie E.; Mashros N.; Mahmud M.Z.H.
Format: Conference paper
Language:English
Published: American Institute of Physics Inc. 2023
Online Access:https://www.scopus.com/inward/record.uri?eid=2-s2.0-85160513069&doi=10.1063%2f5.0113687&partnerID=40&md5=dd338ed8a5040c6a04eef97a382eed88
Description
Summary:Permeable pavement is a form of concrete pavement with a high porosity that allows water from precipitation and other sources to pass through directly, decreasing runoff and permitting groundwater recharging. It is used for concrete flatwork applications. The aim of this study is to evaluate the performance of permeable concrete containing Recycled Coarse Aggregate (RCA), determine the optimum replacement of RCA and study its image characteristic. RCA is the coarse aggregate obtained from the Reclaimed Asphalt Pavement (RAP) that the bitumen content inside it has been extracted. The method used to evaluate the aggregate was bitumen extraction, aggregate crushing value (ACV) and aggregate impact value test (AIV). For pavement concrete mixture was evaluate through compressive strength, flexural strength, porosity, and skid resistance test where image analysis used to characteristic the specimen. Generally, permeable concrete sample containing RCA had the similar compressive strength and exceed the flexural strength when compared to the conventional porous concrete. However, the strengths have a decreasing value with the increase of RCA percentage. On the other hand, for porosity, the percentage increases when the RCA percentage was also increasing. Finally, the skid resistance value is higher than 35 in the dry and wet conditions. © 2023 American Institute of Physics Inc.. All rights reserved.
ISSN:0094243X
DOI:10.1063/5.0113687