Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor
The effects of Li substitution for Sr in (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 (Tl-1212) with x = 0 - 0.10 were investigated. Tl-1212 superconductor pellets were prepared via solid-state reaction and precursor method. The samples were characterized by x-ray diffraction and four-point probe methods. The XRD...
Published in: | Journal of Physics: Conference Series |
---|---|
Main Author: | |
Format: | Conference paper |
Language: | English |
Published: |
Institute of Physics Publishing
2018
|
Online Access: | https://www.scopus.com/inward/record.uri?eid=2-s2.0-85054413796&doi=10.1088%2f1742-6596%2f1083%2f1%2f012033&partnerID=40&md5=b8b73fc49f85e57c1e9e337abe15a609 |
id |
2-s2.0-85054413796 |
---|---|
spelling |
2-s2.0-85054413796 Nur-Akasyah J.; Muhammad Aizat K.; Mohd Suib N.R.; Abd-Shukor R. Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor 2018 Journal of Physics: Conference Series 1083 1 10.1088/1742-6596/1083/1/012033 https://www.scopus.com/inward/record.uri?eid=2-s2.0-85054413796&doi=10.1088%2f1742-6596%2f1083%2f1%2f012033&partnerID=40&md5=b8b73fc49f85e57c1e9e337abe15a609 The effects of Li substitution for Sr in (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 (Tl-1212) with x = 0 - 0.10 were investigated. Tl-1212 superconductor pellets were prepared via solid-state reaction and precursor method. The samples were characterized by x-ray diffraction and four-point probe methods. The XRD patterns showed that all samples formed mixed phases of Tl-1212 and Ca0.3Sr0.7CuO2 (CSCO). The temperature-dependent resistance measurements showed metallic-behavior for all samples with onset transition temperature, Tc onset between 96 K and 105 K and zero resistance temperature, Tc zero between 85 K and 94 K. The transition-width, ΔTc of all samples was in the range of 4 K to 11 K. The x = 0.02 and 0.07 sample showed increase in Tc onset to 105 K and 102 K, respectively. This work showed that Li improved the transition temperature for x = 0.02 and 0.07 samples although the dominant phase was not Tl-1212. © Published under licence by IOP Publishing Ltd. Institute of Physics Publishing 17426588 English Conference paper All Open Access; Gold Open Access |
author |
Nur-Akasyah J.; Muhammad Aizat K.; Mohd Suib N.R.; Abd-Shukor R. |
spellingShingle |
Nur-Akasyah J.; Muhammad Aizat K.; Mohd Suib N.R.; Abd-Shukor R. Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
author_facet |
Nur-Akasyah J.; Muhammad Aizat K.; Mohd Suib N.R.; Abd-Shukor R. |
author_sort |
Nur-Akasyah J.; Muhammad Aizat K.; Mohd Suib N.R.; Abd-Shukor R. |
title |
Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
title_short |
Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
title_full |
Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
title_fullStr |
Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
title_full_unstemmed |
Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
title_sort |
Electrical Properties of Li Substituted (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 Superconductor |
publishDate |
2018 |
container_title |
Journal of Physics: Conference Series |
container_volume |
1083 |
container_issue |
1 |
doi_str_mv |
10.1088/1742-6596/1083/1/012033 |
url |
https://www.scopus.com/inward/record.uri?eid=2-s2.0-85054413796&doi=10.1088%2f1742-6596%2f1083%2f1%2f012033&partnerID=40&md5=b8b73fc49f85e57c1e9e337abe15a609 |
description |
The effects of Li substitution for Sr in (Tl0.85Cr0.15)Sr2-xLixCaCu2O7 (Tl-1212) with x = 0 - 0.10 were investigated. Tl-1212 superconductor pellets were prepared via solid-state reaction and precursor method. The samples were characterized by x-ray diffraction and four-point probe methods. The XRD patterns showed that all samples formed mixed phases of Tl-1212 and Ca0.3Sr0.7CuO2 (CSCO). The temperature-dependent resistance measurements showed metallic-behavior for all samples with onset transition temperature, Tc onset between 96 K and 105 K and zero resistance temperature, Tc zero between 85 K and 94 K. The transition-width, ΔTc of all samples was in the range of 4 K to 11 K. The x = 0.02 and 0.07 sample showed increase in Tc onset to 105 K and 102 K, respectively. This work showed that Li improved the transition temperature for x = 0.02 and 0.07 samples although the dominant phase was not Tl-1212. © Published under licence by IOP Publishing Ltd. |
publisher |
Institute of Physics Publishing |
issn |
17426588 |
language |
English |
format |
Conference paper |
accesstype |
All Open Access; Gold Open Access |
record_format |
scopus |
collection |
Scopus |
_version_ |
1809677906614419456 |